321 inoxidabil oțel țeavă proprietăți și caracteristici

321 inoxidabil oțel țeavă proprietăți și caracteristici

 

TP 321 is a stabil inox oțel whose main advantage is its excelent rezistență la intergranular coroziune după expunere la crom carbură precipitații temperaturi variind de la 800 grad F la 1500 grad F (427 grad la 816 grad ). Aliaj 321 inox oțel tub este stabilizat la formă crom carbură prin adăugare titan.

321 stainless steel pipe properties and characteristics

321 321H Stainless steel is a titanium-stabilized version of 304 for specific applications in the sensitization temperature range. Its resistance to sensitization, coupled with its higher strength at high temperatures, makes it suitable for applications where 304 will be sensitized or 304L thermal strength is insufficient. Weld rot intergranular corrosion does not occur when exposed to a mildly corrosive environment. However, welding 321 should never be used in a highly oxidized environment, as it is susceptible to "knife line" erosion. However, in operating temperatures of more than 500 degree C, the 321 is a better choice and therefore has its own advantages. Alloy 321 stainless steel pipe due to its good mechanical properties, also conducive to high temperature use. Alloy 321 stainless steel has higher creep and stress fracture characteristics than alloy 304, and alloy 304L in particular can also be considered for sensitive and intergranular corrosion problems.

 

321 321H inoxidabil oțel este practic fabricat of 304 inoxidabil oțel. Ei diferă în asta foarte puțin titan este adăugat. The real difference is lor carbon content. The higher the carbon content, the greater the the yield strength. 321 stainless steel has avantaje in high temperature environments due to its excelent mechanical properties. Compared with 304 alloy, 321 stainless steel has better ductility and stress fracture resistance. În adăugare, 304L cutie și fi utilizat la rezistență sensibilizare și intergranular coroziune.

 

Grad 304L is more readily available in most product forms, so if resistance to post-weld intergranular corrosion is only required, 321 is usually preferred. However, the 304L has a lower thermal strength than the 321, so it is not the best choice if it is required to withstanding environments above about 500 degree .